Nano-crystalline diamond (NCD) coating to improve the performance of cutting tools, as the coating thickness varies, the cutting performance and lifespan of the tool varies because the radius of its cutting edge and coating surface roughness are altered. Therefore, an in-depth analysis on the impact of the variations in coating thickness on the cutting tool abrasion and quality of machined surface is necessary. In this study, two NCD ball endmills were coated with 8 and 12 μm thicknesses, and the tool abrasion and roughness of the machined plane were observed after milling. Furthermore, the morphology of the coated surface and abrased cutting edge were observed using a 3D confocal microscope. Consequently, we observed that individual nodules were formed on the continuous aggregates as the coating thickness increased, which increased the coated surface roughness. The two damage modes of the aggregation determined the dominant abrasion that occurred on the cutting edges of both types of coating thicknesses. Delamination and crater wear caused a sharp increase in the roughness of the machined surface. In summary, the increase in coating thickness delayed the delamination of the coating but increased the roughness of the cutting edge, which reduced the machined surface roughness.
An Intrinsic Feedback Capacitor Instrumentation Amplifier (IFCIA) is presented for bio-potential recording and respiratory monitoring. Exploiting the intrinsic gate-to-drain capacitor to scale down input capacitor, combined with interdigitated MOM capacitors, the inverter-based instrumentation amplifier (IA) occupies smallest active area of 0.012 mm2 with 1.5 G Ω input impedance (> > 1G Ω up to 100 Hz) and 0.65 μ A current consumption, while maintaining die-to-die gain mismatch of 0.41%.
The high-purity G5 graphite material is widely used for glass moulding and provides high hardness and brittleness because it is sintered to fine particles unlike other graphite materials. Hence, tool cutting of a G5 workpiece is performed by local fracture instead of plastic deformation of the machined surface. Although a diamond-coated tool with outstanding hardness is used to machine very hard graphite, the tool shows variability regarding the service life and machining performance depending on the grain size, even in the same machining environment. We investigated the wear and change trend of machined surface roughness considering microcrystalline diamond (MCD) and nanocrystalline diamond (NCD)-coated tools, which are generally used to machine graphite materials, and analysed their relation with coating. For rough machining, the MCD-coated tool, for which the delamination of coating occurred later, showed less wear and improved machined surface roughness. For precision machining, the NCD tool showed less tool wear rate relative to the cutting length, leading to a small difference in the machined surface roughness between the two tools. We conclude that if rough and precision machining processes are performed using the same cutting tool, the MCD-coated tool is advantageous in terms of service life, while the difference in roughness of the final machined surface between the tools is negligible.
The domain of edge displays with 2.5D or 3D curved designs has been expanded to improve user convenience. The currently available 3D cover glass offers a limited curvature radius of at least 5 mm and a curvature less than 88°, due to limitations in the undercuts and formability of parts. The development of a full 3D cover, applicable to next-generation displays, requires cover glass molding technology with a curvature exceeding 90°. Here, a mold design and molding process, which addresses the current limitations by dividing the existing glass molding press (GMP) process into two stages, is proposed. The bending geometry of the glass prepared on the basis of the proposed mold design plan during single-step compression forming and two-step compression forming was predicted using commercial analysis software. A molding product with a curvature radius of 2.5 mm and an angle of curvature of 138.9° was produced when process conditions with bending by up to 180° with no damage were applied during actual forming experiments. Further research on annealing and cooling processes of GMP is expected to enable the design and process implementation to manufacture curved glass with a single curvature of at least 90° and multiple curvatures.
The conventional method of making a phosphor layer on the LED package by using a dispensing method is difficult to implement the specific color coordinate, color temperature and optical efficiency because the thickness of the phosphor layer is non-uniform due to precipitation of the phosphor. Besides, the dispensing method consume a large amount of phosphor and silicone to fill the LED package. Thus, studies that manufacture phosphor layer with a uniform thickness such as spray coating, screen printing, electrophoresis are active recently. The purpose of this study is to perform the basic research about the change of the characteristics of phosphor film that is molded with uniform thickness using the phosphor slurry according to various silicone resin and phosphor composition ratio. It is expected to be used as useful information for the fabricating properties when production environment of phosphor layer is changed dispensing method into phosphor film fabrication. In the experiment, it was selected three kinds of methyl-phenyl silicone based resin as the phosphor slurry constituents, and mixed with phosphor various amount of 20 ∼ 60wt% content per one silicone resin. Using this mixed phosphor slurry, it was molded the phosphor film with 300 μm thickness and analyzed the mechanical properties and optical properties of the phosphor film. Finally, the results of this study are presented below: (a) As the phenyl group content is increased, the total heat of reaction need to cure the silicone resin is decrease, and also lower the durometer hardness of the phosphor sheet. On the other hand, it was confirmed that there is no relationship between the phenyl group content in the phosphor film and optical characteristics of the phosphor film. (b) If the amount of the phosphor within the film are increased, then the values of shore hardness and CIE color coordinates are increased gradually but the value of CIE color temperature is decreased gradually in case of being applied same silicone resin to the phosphor film.