26 July 2018 in Metals
Verified
Journal Article
Open access
PDF file
Lenka KucharikovaLenka Kucharikova
Lenka Kucharikova
TLTatiana Liptáková
Tatiana Liptáková
ETEva Tillová
Eva Tillová
DKDaniel Kajánek
Daniel Kajánek
ESEva Schmidova
Eva Schmidova
Aluminum alloys are the most important part of all shaped castings manufactured, especially in the aerospace and automotive industries. This work focuses on the corrosion properties of the heat-hardening aluminum alloys commonly used for production of automotive castings AlSi7Mg0.3 and on self-hardening AlZn10Si8Mg. Iron is a common impurity in aluminum cast alloy and its content increases by using secondary aluminum alloys. Therefore, experimental materials were developed, with chemical composition according to standards (primary alloys) and in states with an increasing content of Fe. The experimental aluminum alloys are briefly discussed in terms of their chemical composition, microstructure, mechanical properties and corrosion behavior. Corrosion properties were examined using three types of corrosion tests: exposure test, potentiodynamic tests, and Audi tests. Corrosion characteristics of materials were evaluated using stereo, optical and scanning electron microscopy, energy dispersive X-ray analysis, too. Correlation of pit initiation sites with microstructural features revealed the critical role of iron-rich phases, silicon particles and corresponding alloy matrix.

1 December 2011 in Manufacturing Technology
Verified
Journal Article
Open access
PDF file
ETEva Tillová
Eva Tillová
MCMária Chalupová
Mária Chalupová
LHLenka Hurtalová
Lenka Hurtalová
EĎEmília Ďuriníková
Emília Ďuriníková
Using recycled aluminium cast alloys is profitable in many aspects. Secondary aluminium produced from recycled metal requires only 2.8 kWh/kg of metal produced and creates only about 5 % as much CO2 as by primary production. Improved mechanica...

13 April 2021 in Materials
Verified
Journal Article
Open access
PDF file
Lenka KucharikovaLenka Kucharikova
Lenka Kucharikova
Denisa StrakováDenisa Straková
Denisa Straková
ETEva Tillová
Eva Tillová
JBJuraj Belan
Juraj Belan
MKMichaela Kritikos
Michaela Kritikos
MUMilan Uhríčik
Milan Uhríčik
Secondary-cast aluminum alloys have increasing industrial applications. Their biggest deficiency is their impurity content, especially Fe, which has low solubility in Al and almost all the content creates intermetallic phases. This work examines the effect of higher Fe content on the microstructure and properties of A356.0 alloy. At the same time, no other possibility existed to affecting the brittleness of the formation of the β phases. The calculation of Fecrit, ratio of Mn/Fe, quantitative and computed tomography analysis of porosity and Fe plate-like phases, measurement of mechanical and fatigue properties, and fractography analysis were performed in this study. The results show that gravity die casting into a sand mold, and the non-usage of Mn addition or heat treatment, do not have a negative effect on increasing the size of the Fe-rich plate-like phases. The longest Fe-rich phases have limited the pore growth and ratios, but their higher thickness led to greater porosity formation. The mechanical and fatigue properties correlate with the Fecrit level and the highest were for the experimental alloy with 0.454 wt.% of Fe. The experimental results confirmed the fact that if the Fe plate-like phases have a length of up to 50 µm, the fatigue properties depend more on the size of porosity. If the length of the Fe needles is more than 50 µm, then the properties are mainly affected by the length of these Fe phases.

1 January 2008 in Strength of Materials
Verified
Journal Article
Closed access
PDF file
MPM. Panušková
M. Panušková
ETEva Tillová
Eva Tillová
MCMaria Chalupova
Maria Chalupova

1 March 2013 in Manufacturing Technology
Verified
Journal Article
Open access
PDF file
LHLenka Hurtalová
Lenka Hurtalová
ETEva Tillová
Eva Tillová
Improved mechanical properties of secondary alloys are strongly dependent upon the morphologies, type and distribution of the second phases, which are in turn a function of alloy composition and cooling rate. In Al-Si-Cu type alloys, however, ...

10 September 2019 in Advances in Materials Science and Engineering
Verified
Journal Article
Open access
JBJuraj Belan
Juraj Belan
Lenka KucharikovaLenka Kucharikova
Lenka Kucharikova
ETEva Tillová
Eva Tillová
MCMaria Chalupova
Maria Chalupova
A polycrystalline alpha-beta TiAl6V4 alloy in the annealed condition was used for the three-point bending fatigue test at frequencyf∼100 Hz. The static preloadFstat. = −15 kN and variable dynamic forceFdyn. = −7 kN to −13.5 kN were set as fatigue test loading parameters. The fatigue life S-N curve presented the stress amplitudeσaas a function of a number of cycles to fractureNf. A limiting number of cycles to run out of 2.0 × 107cycles were chosen for the 3-point fatigue tests of rectangular specimens. In addition, the Smith diagram was used to predict the fatigue life. The alpha lamellae width has a significant influence on fatigue life. It is assumed that the increasing width of alpha lamellae decreases fatigue life. A comparison of fatigue results with given alpha lamellae width in our material to the results of other researchers was performed. The SEM fractography was performed with an accent to reveal the initiation sites of crack at low and high load stresses and mechanism of crack propagation for the fatigue part of fracture.