Red micro-light-emitting diodes (μLEDs) have been generated significant interest for the next generation μLEDs displays. It has been shown that the external quantum efficiency (EQE) of AlInGaP red μLEDs markedly decreases as the size goes to very small dimension. Here, we demonstrate size-independent peak EQE of 611 nm InGaN red μLEDs. Packaged μLEDs show a peak EQE varied from 2.4% to 2.6% as the device area reduces from 100 × 100 to 20 × 20 μm2. These results demonstrate the promising potential for realizing high efficiency red μLED with very small size using InGaN materials.
We present efficient red InGaN 60 × 60 μm2 micro-light-emitting diodes (μLEDs) with an epitaxial tunnel junction (TJ) contact. The TJ was grown by metal-organic chemical vapor deposition using selective area growth. The red TJ μLEDs show a uniform electroluminescence. At a low current density of 1 A/cm2, the emission peak wavelength is 623 nm with a full-width half maximum of 47 nm. The peak external quantum efficiency (EQE) measured in an integrating sphere is as high as 4.5%. These results suggest a significant progress in exploring high efficiency InGaN red μLEDs using TJ technology.
We study the high-temperature electroluminescence properties of 600 nm InGaN red 40 × 40 μm2 micro-light-emitting diodes (μLEDs) with a peak external quantum efficiency (EQE) of 3.2%. Temperature-dependent peak wavelength measurements show a low redshift of 0.05 nm/K. The injection efficiency improves with increasing temperature. The hot/cold (HC) factor is used to quantify the thermal droop: at 400 K, the EQE and wall-plug efficiency HC factors at 50 A/cm2 reach high values of 0.72 and 0.85, respectively. This demonstrates the robustness of InGaN red μLEDs up to high temperature, with a much-improved stability over conventional AlInGaP red μLEDs.
High performance InGaN micro-size light-emitting diodes (µLEDs) with epitaxial tunnel junctions (TJs) were successfully demonstrated using selective area growth (SAG) by metalorganic chemical vapor deposition (MOCVD). Patterned n + GaN/n-GaN layers with small holes were grown on top of standard InGaN blue LEDs to form TJs using SAG. TJ µLEDs with squared mesa ranging from 10×10 to 100×100 µm2 were fabricated. The forward voltage (Vf) in the reference TJ µLEDs without SAG is very high and decreases linearly from 4.6 to 3.7 V at 20 A/cm2 with reduction in area from 10000 to 100 µm2, which is caused by the lateral out diffusion of hydrogen through sidewall. By contrast, the Vf at 20 A/cm2 in the TJ µLEDs utilizing SAG is significantly reduced to be 3.24 to 3.31 V. Moreover, the Vf in the SAG TJ µLEDs is independent on sizes, suggesting that the hydrogen is effectively removed through the holes on top of the p-GaN surface by SAG. The output power of SAG TJ µLEDs is ∼10% higher than the common µLEDs with indium tin oxide (ITO) contact.
InGaN-based red micro-size light-emitting diodes (μLEDs) have become very attractive. Compared to common AlInGaP-based red µLEDs, the external quantum efficiency (EQE) of InGaN red µLEDs has less influence from the size effect. Moreover, the InGaN red µLEDs exhibit a much more robust device performance even operating at a high temperature of up to 400 K. We review the progress of InGaN red μLEDs. Novel growth methods to relax the strain and increase the growth temperature of InGaN red quantum wells are discussed.
A novel approach to realize DFB gratings on GaN based laser diodes is presented and continuous-wave single longitudinal mode operation is achieved. The first order gratings were fabricated on the surface of indium tin oxide (ITO) on top of the laser ridge, which combines the benefits of simplified fabrication, easy scalability to wider ridges, and no regrowth or overgrowth. Under continuous-wave operation, the laser emits with a full FWHM of 5 pm, a SMSR of 29 dB and output power from a single facet as high as 80 mW. To the best of authors’ knowledge, this is also the first demonstration of a DFB-LD on semipolar InGaN/GaN system.