One of the key problems in the billet and shaped casting of aluminum alloys is the presence of various undesirable inclusions and impurities in the melt, which can serve as stress concentrators in the finished product, as well as dissolved hydrogen, which contributes to the formation of porosity. The interaction of aluminum with other gases produced by the combustion of fuel particles, oil, and paint materials brought into the furnace together with charge and scrap increases the amount of nitrides, oxides, carbides, and sulfides in the melt. Flux treatment is widely used as protection of aluminum alloys from oxidation and removal of impurities. The present paper reports the data of a comparative analysis of five widely used flux compositions based on sodium, potassium, and magnesium chlorides. The study covers the following aspects: chemical composition, moisture content, melting temperature and melting range, particle size distribution, and refining ability as measured by the change in Na, Ca, and H2 content after melt treatment.
The paper presents the results of the power parameters when producing rods and wires with Ø 2 mm from them and the mechanical and electrical properties of the resulting semi - finished products from an alloy of the Al - Ce - La system with a rare earth metal content of 1 %. The wire is produced using the method of combined rolling-extrusion (CRE) from the billet Ø 12 mm after electromagnetic mold (EMM), and further drawing. The results of experimental studies of the process of producing longish deformed semi-finished products from the Al - 1 % REM alloy using the CRE-200 combined processing unit are presented. Data were obtained on the mechanical properties of hot - extruded rods Ø 5 mm and Ø 9 mm, as well as wire Ø 2 mm obtained from these rods after implementing the combined processes of rolling - extrusion. It was found that the proposed processing modes make it possible to obtain rods with Ø 9 mm and Ø 5 mm using a combined rolling - extrusion method from workpieces after EMM with diameter 12 mm. The forces on the rolls and die were measured during the implementation of the investigated combined processes. The plasticity of the resulting rods Ø 5 and 9 mm after the CRE method was quite high (elongation to failure reached 14 - 26 %). When drawing wire up to Ø 2 mm, no intermediate annealing was required. The values of electrical resistance do not exceed 0.0271 Ω mm2 m-1 for rods and from 0.0301 Ω mm2 m-1 for wire with a diameter of 2 mm, depending on the processing modes. At all stages of the experimental studies, the structure of the metal was studied and the patterns of change in physical and mechanical properties depending on the processing modes were established.
The depletion of natural resources remains an acute global problem, highlighting the importance of developing sustainable technologies that enable the simultaneous extraction of metals and recycling of waste. This paper describes a study of a technology for recycling aluminum slag from foundries to produce secondary aluminum alloy and regenerated flux. Research and processing methods include X-ray phase and spectral analysis of slag composition, multi-stage grinding in a jaw crusher and planetary mill, screening for fraction separation, and selective dissolution of the oxide–salt phase in water or hydrochloric acid followed by filtration and evaporation; obtaining regenerated flux based on phase diagrams of chloride systems; and briquetting and remelting of the extracted aluminum. The technology ensures the extraction of up to 85% of the metallic aluminum from slag and the production of regenerated flux based on the NaCl–KCl–MgCl2 system with a low melting point.