Elvira Akhmetova

Ms. Elvira Akhmetova

orcid

Research Focus & Metrics

Academic Career Length

1Year (2026-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
29 March 2026 in Bulletin of the Karaganda University "Physics Series"
Verified
Journal Article
Closed access
Aidar KengesbekovAidar Kengesbekov
Aidar Kengesbekov
AZAinur Zhassulan
Ainur Zhassulan
NMNazerke Muktanova
Nazerke Muktanova
DBDaryn Baizhan
Daryn Baizhan
EAElvira Akhmetova
Elvira Akhmetova
ASA. Serikbaikyzy
A. Serikbaikyzy
Titanium and its alloys are widely used in biomedical implants due to their favorable mechanical properties and corrosion resistance; however, their natural surface lacks sufficient bioactivity. Micro-arc oxidation is a promising approach to producing bioactive coatings, and the incorporation of nanoparticles such as TiO2 may further improve their functionality. This study aimed to determine the optimal TiO2 nanoparticle concentration in the micro-arc oxidation electrolyte that ensures coating stability and biological safety. Calcium–phosphate coatings were fabricated on commercially pure titanium using micro-arc oxidation with two TiO2 concentrations: 0.5 wt.% (MAO 1) and 1 wt.% (MAO 2). Surface morphology, porosity, and phase composition were analyzed by scanning electron microscopy, energy-dispersive spectroscopy, and X-ray diffraction. Corrosion resistance was evaluated via potentiodynamic polarization in NaCl and Ringer’s solutions, while biocompatibility was assessed in vitro using HOS human osteosarcoma cells and MTT assays. Increasing the TiO2 content to 1 % decreased coating porosity (13.7 % vs. 26.3 % for MAO 1), enhanced corrosion protection, and reduced the friction coefficient compared to bare titanium. However, MAO 2 exhibited high cytotoxicity (81 % cell death) and partial structural degradation in the biological medium. MAO 1 maintained integrity and showed no toxic effects (3 % cell death). These results suggest that 0.5 % TiO2 is the optimal concentration, providing a balance between corrosion resistance, mechanical stability, and biocompatibility, supporting the development of safer implant coatings.

3 July 2026 in Coatings
Verified
Journal Article
Open access
PDF file
BRBauyrzhan Rakhadilov
Bauyrzhan Rakhadilov
Aidar KengesbekovAidar Kengesbekov
Aidar Kengesbekov
EAElvira Akhmetova
Elvira Akhmetova
AAArnur Askhatov
Arnur Askhatov
This study investigates titanium oxynitride (TiOxNy) coatings deposited by reactive magnetron sputtering on 316L stainless steel substrates in an Ar–N2–O2 gas mixture at a fixed N:O ratio of 1.6. The coatings were deposited under three reactive magnetron sputtering regimes with Ar flow rates of 33, 28, and 26 sccm and corresponding substrate biases of −50, −100, and −150 V, respectively, while the N2 and O2 flow rates were kept constant at 10 and 6 sccm. The coatings exhibited a dense microstructure, with thicknesses ranging from 2.13 to 5.51 μm. X-ray diffraction analysis revealed the formation of a multiphase structure comprising TiN, TiOxNy, and TiO. The deposition regime had a significant influence on the functional properties of the coatings. The lowest friction coefficients (µ ≈ 0.26–0.28) and stable tribological behavior were characteristic of the Ar26 sample. The highest corrosion resistance was observed for the Ar28 sample, with a corrosion current density of icorr = 2.82 × 10−7 A/cm2 and a corrosion rate of vcorr = 0.00573 mm/year. All coatings exhibited hydrophilic surface behavior, with contact angles of 50–57°, which may be relevant for further evaluation in biomedical surface applications. Thus, the structure and functional properties of TiOxNy coatings can be regulated by selecting an appropriate deposition regime, including the Ar flow rate, relative reactive gas fraction, and substrate bias. However, additional biological tests, including cytotoxicity, hemocompatibility, endothelialization, and platelet adhesion studies, are required before conclusions about vascular implant applicability can be made.

2 November 2026 in Coatings
Verified
Journal Article
Open access
PDF file
BRBauyrzhan Rakhadilov
Bauyrzhan Rakhadilov
Aidar KengesbekovAidar Kengesbekov
Aidar Kengesbekov
UIUmar Ibtasam
Umar Ibtasam
NMNurtoleu Magazov
Nurtoleu Magazov
EAElvira Akhmetova
Elvira Akhmetova
Suresh AlapatiSuresh Alapati
Suresh Alapati
Atmospheric plasma-sprayed FeCrAl coatings possess heterogeneous lamellar structures whose characterization is important for interpreting friction and wear. This study compared four as-sprayed FeCrAl coatings produced at nominal powder feed rates of 25–40 g/min and a common stand-off distance of 150 mm. The objective was to compare their microstructural and surface characteristics with their room-temperature dry-sliding responses, particularly the correspondence between friction and wear rankings. The coatings were examined using SEM/EDS, X-ray diffraction, cross-sectional image analysis, surface profilometry, instrumented indentation, and ball-on-disk testing. Mean coating thicknesses ranged from 162 to 702 µm, while region-specific apparent porosity estimates ranged from 0.38 to 1.49%. The coatings exhibited heterogeneous lamellar microstructures and broadly similar diffraction patterns dominated by an α-Fe-type bcc matrix containing Cr, with additional reflections assigned to Fe3O4. The mean Ra values ranged from 22.83 ± 0.13 to 26.91 ± 0.36 µm (mean ± SD, n = 3), and individual indentations revealed substantial variation in local mechanical response. F3 exhibited the lowest measured specific wear rate of 1.051 × 10−4 mm3/(N·m) among the tested specimens. F4 showed the lowest approximate post-running-in friction coefficient of 0.77–0.80, whereas F1 exhibited the highest measured specific wear rate of 1.982 × 10−4 mm3/(N·m). Thus, the friction and wear rankings differed, and neither the measured roughness nor the region-specific apparent porosity alone accounted for the wear ranking. These findings characterize the tested specimens; one sliding test per coating and incomplete deposition records preclude establishing reproducibility or attributing the differences exclusively to powder feed rate.

15 October 2026 in Lubricants
Verified
Journal Article
Open access
PDF file
BRBauyrzhan Rakhadilov
Bauyrzhan Rakhadilov
NMNurtoleu Magazov
Nurtoleu Magazov
Aidar KengesbekovAidar Kengesbekov
Aidar Kengesbekov
Małgorzata RutkowskaMałgorzata Rutkowska
Małgorzata Rutkowska
DKDauir Kakimzhanov
Dauir Kakimzhanov
EAElvira Akhmetova
Elvira Akhmetova
WC-12Co coatings deposited by liquid-fuel high-velocity oxy-fuel (HVOF) spraying at kerosene pump frequencies of 33, 35, and 37 Hz were evaluated by cross-sectional scratch testing at 5–25 N and dry sliding at a constant load of 10 N. F35 exhibited the highest mean Martens hardness (9.42 GPa), whereas F33 had the smallest mean projected scratch-damage area at 5–15 N. On ground surfaces, F35 showed the lowest specific wear rates in reciprocating and ball-on-disc tests: 3.61 × 10−6 and 5.69 × 10−5 mm3 N−1 m−1, respectively. For the as-sprayed surface under reciprocating sliding, the lowest value was obtained for F37. Wear results represent one test per coating in each configuration. SEM/EDS observations were consistent with local material removal, transfer from the steel counterbody, and the formation of oxygen-enriched regions. The different rankings obtained from hardness, scratch damage, and wear measurements show that the coating response depends on the deformation scale and contact conditions.

24 June 2026 in Journal of Surface Engineering and Coating Technology
Verified
Journal Article
Open access
EAElvira Akhmetova
Elvira Akhmetova
Aidar KengesbekovAidar Kengesbekov
Aidar Kengesbekov
ASAlmira Serikhan
Almira Serikhan
TiON coatings were deposited on 316L stainless steel substrates by reactive magnetron sputtering under three different deposition regimes. The study aimed to determine the optimal sputtering conditions by comparing the mechanical properties, elemental composition, and corrosion behavior of the coatings. Instrumented indentation showed that the deposition regime strongly affected the mechanical response of the coatings. The highest hardness and elastic modulus were obtained for sample R3, reaching 639.3 HV and 152.6 GPa, respectively. SEM observations confirmed the formation of continuous coating layers, while EDS analysis revealed changes in elemental composition depending on the sputtering regime. The oxygen content decreased from R1 to R3, while nitrogen was detected only in the R3 coating. Electrochemical tests in 3.5 wt.% NaCl solution showed that R1 exhibited the lowest corrosion current density of 1.13 × 10⁻⁷ A/cm² and the lowest corrosion rate of 0.00231 mm/year. R3 demonstrated intermediate corrosion

30 September 2026 in Science and Technology of Kazakhstan
Verified
Journal Article
Closed access
БРБ. К. Рахадилов
Б. К. Рахадилов
NMNazerke Muktanova
Nazerke Muktanova
EAElvira Akhmetova
Elvira Akhmetova
NMNurtoleu Magazov
Nurtoleu Magazov
Цель работы заключалась в получении однослойных покрытий CrN и многослойных покрытий Cr/CrN на циркониевом сплаве E110 и в оценке влияния газового режима осаждения и многослойной архитектуры на их структурное состояние, механико-трибологические свойства и устойчивость к высокотемпературному паровому окислению. Покрытия получали реактивным магнетронным распылением хромовой мишени. Для однослойного CrN проверяли три газовых режима Ar/N2 : 90/30, 85/35 и 80/40 ст.см³/мин. Для Cr/CrN готовили покрытия из 2, 4 и 6 слоёв. Образцы исследовали методами СЭМ/EDS, XRD, GDOES, наноиндентирования, АСМ и испытаний на трение; отдельно проводили выдержку в водяном паре при 1100 °C в течение 2 ч. Установлено, что при Ar/N2 = 80/40 ст.см³/мин формируется наиболее ровный однослойный CrN: Ra = 0,114±0,006 мкм, а на рентгенограмме выражены линии кубического CrN. В серии Cr/CrN толщина увеличивалась с ростом числа слоёв; у 6-слойного образца она достигала около 4,18 мкм. Для этого покрытия получены H = 5,00±0,27 ГПа, E = 110±4 ГПа и скорость износа 2,26×10-4 мм³·Н-¹·м-¹ После парового окисления на поверхности покрытий регистрировался Cr2 O3 , а в 6-слойном образце сохранялись слабые линии CrN и Cr, что указывает на частичную сохранность внутренних слоёв. Практическая значимость работы состоит в обосновании перспективности многослойной архитектуры Cr/CrN как защитного барьерного покрытия для циркониевых оболочек ТВЭЛ нового поколения, устойчивых к аварийным режимам эксплуатации. Ключевые слова: циркониевый сплав E110, покрытия Cr/CrN, магнетронное распыление, высокотемпературное паровое окисление, многослойная структура, топливо, устойчивое к авариям.