Faculty of Electrical Engineering, Electrotechnical Material Laboratory, University Politehnica of Bucharest, Splaiul Independentei, 313, 060042 Bucharest, Romania
Dr. Cristina STANCU
Faculty of Electrical Engineering, Electrotechnical Material Laboratory, University Politehnica of Bucharest, Splaiul Independentei, 313, 060042 Bucharest, Romania
Electrical properties and electro-thermal behavior were studied in composites with carbon black (CB) or hybrid filler (CB and graphite) and a matrix of linear low-density polyethylene (LLDPE). LLDPE, a (co)polymer with low crystallinity but with high structural regularity, was less studied for Positive Temperature Coefficient (PTC) applications, but it would be of interest due to its higher flexibility as compared to HDPE. Structural characterization by scanning electron microscopy (SEM) confirmed a segregated structure resulted from preparation by solid state powder mixing followed by hot molding. Direct current (DC) conductivity measurements resulted in a percolation threshold of around 8% (w) for CB/LLDPE composites. Increased filler concentrations resulted in increased alternating current (AC) conductivity, electrical permittivity and loss factor. Resistivity-temperature curves indicate the dependence of the temperature at which the maximum of resistivity is reached (Tmax(R)) on the filler concentration, as well as a differentiation in the Tmax(R) from the crystalline transition temperatures determined by DSC. These results suggest that crystallinity is not the only determining factor of the PTC mechanism in this case. This behavior is different from similar high-crystallinity composites, and suggests a specific interaction between the conductive filler and the polymeric matrix. A strong dependence of the PTC effect on filler concentration and an optimal concentration range between 14 and 19% were also found. Graphite has a beneficial effect not only on conductivity, but also on PTC behavior. Temperature vs. time experiments, revealed good temperature self-regulation properties and current and voltage limitation, and irrespective of the applied voltage and composite type, the equilibrium superficial temperature did not exceed 80 °C, while the equilibrium current traversing the sample dropped from 22 mA at 35 V to 5 mA at 150 V, proving the limitation capacities of these materials. The concentration effects revealed in this work could open new perspectives for the compositional control of both the self-limiting and interrupting properties for various low-temperature applications.
25 August 2020 in IEEE Transactions on Components, Packaging and Manufacturing Technology
A rapid method based on activation energy values for the lifetime assessment of PP films used as dielectrics for capacitors is proposed. The activation energy is determined from a nonisothermal measurement made by differential scanning calorimetry and an aging test at a single elevated temperature. The use of the onset temperature of the exothermal peak is proposed to evaluate the activation energy of the degradation of the PP film. Four types of PP film capacitors were thermally aged at 100 °C for different aging times. For each aging time, the capacitance was measured at different frequencies. According to the standards, two end-of-life criteria (2 % and 5 %) were imposed for the reduction of the capacitance. The parameters of the lifetime line a and b were determined, and finally, the lifetime values were calculated. The novel proposed method is effective in terms of both energy and manpower costs compared to the current method, which uses three aging temperatures.
18 August 2016 in IEEE Transactions on Components, Packaging and Manufacturing Technology
One of the most vulnerable components of electronic circuits is the solder joints. The most common technique of soldering used in electronics is the reflow soldering. During the soldering process, different issues may occur leading to the inception of some defects (tombstone effect, flux spattering, etc.). To avoid these defects, it is mandatory to follow the parameter values of the reflow process, especially temperature values. In this paper, the temperature distribution for three types of samples (two interconnected soldering pads-without solder, with solder on one pad, and with solder on both pads) during the reflow soldering process, calculated with Comsol Multiphysics software (heat transfer 3-D module) is presented. The calculated values are then compared to the ones obtained by experiments in order to verify the accuracy of the numerical model. To carry out the computations, the latent heat of melting/solidification and the variation with the temperature of the solder parameters were considered. The results show that there is a good correlation between the measured and calculated values, the differences (for all types of samples) being lower than ±3 °C.
A structural model for the calculation of the equivalent permittivity of nanocomposites based on low-density polyethylene (LDPE) and epoxy resins (ERs) with inorganic fillers was developed. It was assumed that each nanoparticle was centered in an interfacial region composed of three layers in the case of LDPE-based nanocomposites, and of two layers in the case of ER-based nanocomposites. The model for the estimation of the permittivity was designed for flat samples of the height $g$ , divided into cubes with the side-length $l$ . Each of these cubes contains eight nanoparticles, which are separated from the polymer matrix by two or three layers. Based on the types and concentrations of dipoles present in the layers, the relative permittivity of each layer of the interface can be calculated. By the employment of a 3D numerical model in COMSOL, implemented by the finite element method associated with a cube, the distribution of the electric field inside a cube can be determined, which yields the values of the equivalent permittivity of the nanocomposites. In order to verify the numerical results, the permittivity of the nanocomposites based on LDPE and ERs with inorganic nanofillers (SiO 2 or Al 2 O 3 ) was determined in laboratory experiments. The results reveal congruent correlation between the computed and the experimentally determined values of the equivalent permittivity of the nanodielectrics.
Solder is usually an alloy of two and more metals. Very often is used tin, lead, copper, silver, bismuth, nickel, etc. for its production. If the alloy is exposed to a sufficiently high temperature, it is induced phase change from solid to liquid phase for it. Phase is changed again from liquid to solid during cooling substance. At this point, the substance generates a latent heat that is manifests differently for each alloy. Each component contributes its thermal and conductivity parameters into the overall properties of the alloy. The result determines quantity of the generated latent heat. And by final amount of the temperature acts on their surroundings. There have been several experimental measurements for determining of decomposition of temperature in a volume of electrically conductive solder joints during a phase change (from liquid to solidstate). Measurements were carried out on the reference alloy Sn-Pb (eutectic) and three lead-free solder alloys.