The high-temperature oxidation behavior of selective laser melting (SLM) manufactured IN 625 was studied over 96 h of exposure at 900 °C and 1050 °C in air. An extensive analysis was performed to characterize the oxide scale formed and its evolution during the 96 h, including mass gain analysis, EDS, XRD, and morphological analysis of the oxide scale. The mass gain rate of the bare material increases rapidly during the first 8 h of temperature holding and diminishes at higher holding periods for both oxidation temperatures. High-temperature exposure for short periods (24 h) follows a parabolic law and promotes the precipitation of δ phase, Ni-rich intermetallics, and carbides. Within the first 24 h of exposure at 900 °C, a Cr2O3 and a (Ni, Fe)Cr2O4 spinel scale were formed, while at a higher temperature, a more complex oxide was registered, consisting of (Ni, Fe)Cr2O4, Cr2O3, and rutile-type oxides. Prolonged exposure of IN 625 at 900 °C induces the preservation of the Cr2O3 scale and the dissolution of carbides. Other phases and intermetallics, such as γ, δ phases, and MoNi4 are still present. The exposure for 96 h at 1050 °C led to the dissolution of all intermetallics, while the same complex oxide scale was formed.
The present study was focused on the assessment of microstructural anisotropy of IN 625 manufactured by selective laser melting (SLM) and its influence on the material’s room temperature tensile properties. Microstructural anisotropy was assessed based on computational and experimental investigations. Tensile specimens were manufactured using four building orientations (along Z, X, Y-axis, and tilted at 45° in the XZ plane) and three different scanning strategies (90°, 67°, and 45°). The simulation of microstructure development in specimens built along the Z-axis, applying all three scanning strategies, showed that the as-built microstructure is strongly textured and is influenced by the scanning strategy. The 45° scanning strategy induced the highest microstructural texture from all scanning strategies used. The monotonic tensile test results highlighted that the material exhibits significant anisotropic properties, depending on both the specimen orientation and the scanning strategy. Regardless of the scanning strategy used, the lowest mechanical performances of IN 625, in terms of strength values, were recorded for specimens built in the vertical position, as compared with all the other orientations.
Nickel-based superalloys are extensively used in high-temperature applications because of their exceptional oxidation and corrosion resistance. However, their performance in aggressive environments containing molten salts, such as Na2SO4 and V2O5, remains a critical challenge. This study investigated the hot corrosion behavior of Inconel 718, Udimet 710, Nimonic 75, and Inconel 625, focusing on the role of the alloying elements in the corrosion layers and degradation mechanisms. The superalloys were exposed to 50/50 wt.% Na2SO4–V2O5 at 900 °C for 8, 48, and 96 h, and their corrosion resistance was evaluated through weight gain measurements, scanning electron microscopy (SEM), and energy-dispersive X-ray spectroscopy (EDS). These results indicate that Mo is a key factor in accelerating degradation, with Inconel 625 exhibiting the highest weight gain owing to the formation of thermally unstable Mo-rich phases. Fe also negatively impacted the stability of the protective scale of Inconel 718, contributing to an increased corrosion rate. In contrast, Nimonic 75 exhibited the best resistance, forming more of the NiCr2O4 spinel phase through the reaction of Cr2O3 with NiO from the high Ni and Cr contents in the corrosive layers. These findings highlight the importance of alloy composition in optimizing corrosion resistance and suggest that using superalloys with lower Mo and Fe contents and higher Cr and Ni concentrations can significantly enhance the durability of superalloys in molten salt environments.
In this study, a CoCrMo-based metallic alloy was manufactured using a 3D-printing method with metallic powder and a laser-based 3D printer. The obtained material was immersed in a simulated body fluid (SBF) similar to blood plasma and kept 2 months at 37 °C and in relative motion against the SBF in order to mimic the real motion of body fluids against an implant. At determined time intervals (24, 72, 168, 336, and 1344 h), both the metallic sample and SBF were characterized from a physical-chemical point of view in order to assess the alloy’s behaviour in the SBF. Firstly, the CoCrMo based metallic sample was characterized by scanning electron microscopy (SEM) for assessing surface corrosion and X-ray diffraction (XRD) for determining if and/or what kind of spontaneous protective layer was formed on the surface; secondly, the SBF was characterized by pH, electrical conductivity (EC), and inductively coupled plasma mass spectroscopy (ICP-MS) for assessing the metal ion release. We determined that a 3D-printed CoCrMo alloy does not represent a potential biological hazard in terms of the concentration of metal ion releases, since it forms, in a relatively short period of time, a protective CoCr layer on its exposed surface.
Electrical properties and electro-thermal behavior were studied in composites with carbon black (CB) or hybrid filler (CB and graphite) and a matrix of linear low-density polyethylene (LLDPE). LLDPE, a (co)polymer with low crystallinity but with high structural regularity, was less studied for Positive Temperature Coefficient (PTC) applications, but it would be of interest due to its higher flexibility as compared to HDPE. Structural characterization by scanning electron microscopy (SEM) confirmed a segregated structure resulted from preparation by solid state powder mixing followed by hot molding. Direct current (DC) conductivity measurements resulted in a percolation threshold of around 8% (w) for CB/LLDPE composites. Increased filler concentrations resulted in increased alternating current (AC) conductivity, electrical permittivity and loss factor. Resistivity-temperature curves indicate the dependence of the temperature at which the maximum of resistivity is reached (Tmax(R)) on the filler concentration, as well as a differentiation in the Tmax(R) from the crystalline transition temperatures determined by DSC. These results suggest that crystallinity is not the only determining factor of the PTC mechanism in this case. This behavior is different from similar high-crystallinity composites, and suggests a specific interaction between the conductive filler and the polymeric matrix. A strong dependence of the PTC effect on filler concentration and an optimal concentration range between 14 and 19% were also found. Graphite has a beneficial effect not only on conductivity, but also on PTC behavior. Temperature vs. time experiments, revealed good temperature self-regulation properties and current and voltage limitation, and irrespective of the applied voltage and composite type, the equilibrium superficial temperature did not exceed 80 °C, while the equilibrium current traversing the sample dropped from 22 mA at 35 V to 5 mA at 150 V, proving the limitation capacities of these materials. The concentration effects revealed in this work could open new perspectives for the compositional control of both the self-limiting and interrupting properties for various low-temperature applications.
Inconel 625 samples, obtained by Selective Laser Melting (SLM) and conventional technology, were tested for hot corrosion resistance against a molten mixture of Na2SO4 and V2O5. The assessments were performed in air, at 900 °C with exposure time of up to 96 h, and at 1000 °C for 8 h. Weight gain was higher for samples obtained by SLM, with 37.4% after 8 h, 3.98% after 24 h, 4.46% after 48 h, and 5.8% after 96 h at 900 °C (22.6% at 1000 °C, 8 h). Three stages of corrosion were observed, the first and last with a high corrosion rate, while the second one showed a slower corrosion rate. Corrosion behaviour depends on the morphology of the grain boundary, which can influence the infiltration of corrosive salts, and on the formation of Cr2NiO4 compound, which acts as a temporary barrier.