1 May 2016 in Microelectronics Reliability
8 January 2018 in Circuit World
Purpose: The purpose of this paper is to increase the reliability of manufactured electronics and to reveal reliability significant factors. The experiments were focused especially on the influence of the reflow oven parameters presented by a heating factor. Design/methodology/approach: The shear strength of the surface mount device (SMD) resistors and their joint resistance were analyzed. The resistors were assembled with two Sn/Ag/Cu-based and one Bi-based solder pastes, and the analysis was done for several values of the heating factor and before and after isothermal aging. The measurement of thickness of intermetallic compounds was conducted on the micro-sections of the solder joints. Findings: The shear strength of solder joints based on the Sn/Ag/Cu-based solder alloy started to decline after the heating factor reached the value of 500 s · K, whereas the shear strength of the solder alloy based on the Bi alloy (in the measured range) always increased with an increase in the heating factor. Also, the Bi-based solder joints showed shear strength increase after isothermal aging in contrast to Sn/Ag/Cu-based solder joints, which showed shear strength decrease. Originality/value: The interpretation of the results of such a comprehensive measurement leads to a better understanding of the mutual relation between reliability and other technological parameters such as solder alloy type, surface finish and parameters of the soldering process.
25 August 2020 in IEEE Transactions on Components, Packaging and Manufacturing Technology
A rapid method based on activation energy values for the lifetime assessment of PP films used as dielectrics for capacitors is proposed. The activation energy is determined from a nonisothermal measurement made by differential scanning calorimetry and an aging test at a single elevated temperature. The use of the onset temperature of the exothermal peak is proposed to evaluate the activation energy of the degradation of the PP film. Four types of PP film capacitors were thermally aged at 100 °C for different aging times. For each aging time, the capacitance was measured at different frequencies. According to the standards, two end-of-life criteria (2 % and 5 %) were imposed for the reduction of the capacitance. The parameters of the lifetime line a and b were determined, and finally, the lifetime values were calculated. The novel proposed method is effective in terms of both energy and manpower costs compared to the current method, which uses three aging temperatures.
12 February 2019 in Journal of Materials Science: Materials in Electronics
In our paper, the characterization of glass transition temperature (Tg) was performed for one- and two-component electrically conductive adhesive used in electronic joining technologies. Both adhesives were of the epoxy type with the silver filler. Dynamic mechanical analysis (DMA) was used to measure the Tg. The adhesives were modified with nanoparticles, namely, carbon nanotubes (concentration of 0.5 and 0.8% by weight) and silver nanoballs (2.5% by weight). The values of Tg were determined from the plot of the Tg δ parameter. Two types of environmental stresses were used for climatic aging: 125 °C/56% RH and 85 °C/85% RH. The aging of the samples at 125 °C and 56% RH caused increase Tg for all formulations. The cause of these changes is additional curing of adhesive. Aging in the combined climate 85 °C/85% RH caused a shift in Tg toward lower values for formulations based on the one-component adhesive modified by CNT and toward higher values for all other formulations. The major cause of the decrease in Tg was that CNT inhered the curing reactions and banned them from completion. In cases where Tg grew, glue hardening take place. DMA was performed to examine Tg of the samples. The DMA measurements were carried out up to 200 °C. Repeated DMA measurement confirmed that this measurement caused additional hardening and increase Tg for all samples. The results will contribute to the use of conductive adhesives with better quality and reliability in electronics manufacturing.
3 April 2018 in Soldering & Surface Mount Technology
Purpose: The purpose of this paper is to present a novel approach on investigating critical current densities in the solder joints of chip-size surface mounted device (SMD) components. The investigation involves a numerical approach and a physical validation with selected track-to-pad connections and high current loads (CXs). Design/methodology/approach: During the investigations, shape of solder fillets was calculated in Surface Evolver, and then the current densities were calculated accordingly in the given geometry. For the verification, CX tests were performed on joints at elevated temperatures. The joints were qualified with X-ray microscopy, cross-section analysis and shear tests. Findings: This study ascertained that the inhomogeneity in current density depends on the track-to-pad structure of the joint. Also this study found that the heavy CX decreases the mechanical strength, but the degradation does not reach the level of electromigration (EM)-induced voiding. Practical implications: The heavy CX significantly affects joint reliability and the results point out to EM-induced failure-limitations on printed circuit board (PCB)-based assemblies due to the thermomechanical weakness of the FR4 material. Originality/value: The experiments investigate current density from a novel aspect on more frequently used small-scale components with different track-to-pad configurations – pointing out possible failure sources.