With increasing traffic loads and the continuous deterioration of asphalt pavements, it has become necessary to explore alternative materials that enhance both performance and sustainability. This study aims to investigate the effect of using cement kiln dust (CKD) as a filler substitute in hot mix asphalt composites, focusing on the mechanical and durability properties of pavements. The results indicate that replacing conventional filler with CKD in different proportions (1.5%, 3%, 4.5%, and 6%) positively affects the properties of asphalt mixtures. Marshall stability values increased by 58.4% when using 100% CKD, indicating a significant improvement in the mixture’s ability to withstand traffic loads. Flow tests revealed that replacing CKD by up to 50% enhances the flexibility of the mixture, but exceeding this percentage makes the mixture stiffer, which may lead to premature cracking. In terms of moisture sensitivity, incorporating CKD by 25% improves the mixture’s resistance to water damage, while increasing it to 100% reduces this resistance, highlighting the need to improve the adhesion properties of asphalt. Indirect tensile strength tests have confirmed that CKD enhances the cohesion of the mixture, reducing the likelihood of cracking under pressure and contributing to longer pavement life. Based on these results, it is recommended that CKD be used for up to 50% to achieve a balanced combination of strength, flexibility, and moisture resistance, with further studies being needed to evaluate the long-term performance and potential improvements through additional material modifications.
The use of hot mix asphalt (HMA) has several drawbacks, such as the emission of harmful gases into the atmosphere, difficulties in maintaining temperature over long distances, and the requirement for high energy consumption during preparation and installation. In order to solve these issues, this research aimed to produce High-Performance Cold Mix Asphalt (HP-CMA), in which Ordinary Portland Cement (OPC) is used as a filler to replace limestone filler at 0%, 1.5%, 3%, 4.5%, and 6% of the aggregate weight. Indirect Tensile Stiffness Modulus (ITSM), moisture susceptibility, temperature susceptibility, and microstructural analysis tests were carried out. The results showed that the ITSM was considerably enhanced when OPC was utilized. When comparing HP-CMA with 3% OPC to the control HMA (100–150 pen), the ITSM increased by approximately 80% after three days. In contrast, HP-CMA with 4.5% OPC achieved the same ITSM as the control HMA (40–60 pen) after seven days. Moreover, the ITSM of the HMA 40–60 pen decreased by 91.93% when the temperature rose from 20 °C to 45 °C, whereas the ITSM of the HP-CMA with 6% OPC decreased by 42.47% over the same temperature range. This suggests that HP-CMA is more stable than the HMA 40–60 pen at elevated temperatures. The superior performance of the HP-CMA can be attributed to two essential factors: the improved binding effect due to the demulsification of the asphalt emulsion used as a binder, and the formation of hydration products from the added cement.