4 November 2023 in Applied Surface Science
20 December 2022 in IEEE Journal of Photovoltaics
We have studied the mechanisms underpinning effective surface passivation of silicon with hafnium oxide (HfO 2 ) thin films grown via atomic layer deposition (ALD). Plasma-enhanced ALD with O 2 plasma and a tetrakis(dimethylamido)hafnium precursor was used to deposit 12 nm thick HfO 2 films at 200 °C on high-lifetime 5 Ωcm n -type Czochralski silicon wafers. The passivation was activated by postdeposition annealing, with 30 min in air at 475 °C found to be the most effective. High-resolution grazing incidence X-ray diffraction measurements revealed the film crystallized between 325 and 375 °C, and this coincided with the onset of good passivation. Once crystallized, the level of passivation continued to increase with higher annealing temperatures, exhibiting a peak at 475 °C and yielding surface recombination velocities of 475 °C. By superacid repassivation, we demonstrated this reduction in lifetime was not because of a decrease in the bulk lifetime, but rather because of changes in the passivating films themselves. Kelvin probe measurements showed the films are negatively charged. Corona charging experiments showed the charge magnitude is of order 10 12 qcm −2 and that the reduced passivation above 475 °C was mainly because of a loss of chemical passivation. Our study, therefore, demonstrates the development of highly charged HfO 2 films and quantifies their benefits as a standalone passivating film for silicon-based solar cells.
1 June 2023 in AIP Advances
Thin film dielectrics are ubiquitous in the manufacture of electronic devices and are frequently deposited and etched away at various stages of device fabrication. We demonstrate that hafnium oxide (HfO2) thin films grown via atomic layer deposition on silicon and silicon pre-coated with aluminum oxide (Al2O3) have etch resistance properties, which can be tuned simply by changing the post-deposition annealing temperature. The etching rates of films in hydrofluoric acid (HF) solutions were found to be dependent on annealing temperature, with the etch rate decreasing with increasing temperature. A transition region in the etch rate was identified between 300 and 350 °C, corresponding to the crystallization of the HfO2 films, as identified via x-ray diffraction. HfO2 films deposited directly onto silicon annealed above 350 °C were resistant to 10% HF solutions over the course of several hours. In the case of Si/Al2O3/HfO2 stacks, closer inspection reveals the existence of channels, which reduces the etch resistance of HF acid, as evidenced by tetramethylammonium hydroxide etching of the silicon substrate. Crystallized HfO2 can be used to protect other dielectrics in device processing, and we demonstrate its use in single-sided fabrication of patterned structures of Al2O3, which can control the effective charge-carrier lifetime in silicon wafers for use in modulating THz and mm-wave radiation.
16 December 2022 in Journal of Applied Physics
For a diverse range of semiconductor devices, the charge carrier lifetime is an essential characteristic. However, the carrier lifetime is difficult to control, as it is usually determined by a variety of recombination processes. For indirect bandgap materials, it is well known that effective carrier lifetimes can be improved by passivating the surface, effectively extinguishing surface-related recombination processes. However, for some applications, such as photomodulators for sub-infrared radiation, it is beneficial to tailor lifetimes to specific values, in this particular case trading off between photo-efficiency and switching speed. In this paper, we design a new type of silicon-based metamaterial with a tunable electron–hole lifetime. By periodically patterning a dielectric surface passivation layer, we create a metamaterial whereby the filling fraction of passivated relative to unpassivated areas dictates the effective charge carrier lifetime. We demonstrate tunable lifetimes between 200 μs and 8 ms in a 670 μm thick Si wafer, though in principle our approach allows one to generate any lifetime between the fully passivated and unpassivated limits of a bulk semiconductor. Finally, we investigate the application of these metamaterials as photomodulators, finding switching times that depend upon both the photoexcitation intensity, wafer thickness, and the carrier lifetime.
11 July 2023 in IEEE Journal of Photovoltaics
Minimizing electrical losses at metal/silicon interfaces in high-efficiency single-junction silicon solar cells requires the use of carrier-selective passivating contacts. The electronic barrier heights at the insulator/silicon interface are necessary for calculating the probability of quantum tunneling of charge carriers at these interfaces. Thus, precise knowledge of these parameters is crucial for the development of contact schemes. Using a photoemission-based method, we experimentally determine the electronic band offsets of Al 2 O 3 , HfO 2 and SiO 2 layers grown by atomic layer deposition (ALD) on silicon. For Al 2 O 3 /Si, we determine a valence band offset (Δ EV ) and conduction band offset (Δ EC ) of 3.29 ± 0.07 eV and 2.24 ± 0.13 eV, respectively. For HfO 2 /Si, Δ EV and Δ EC are determined as 2.67 ± 0.07 eV and 1.81 ± 0.21 eV, while for SiO 2 /Si, Δ EV and Δ EC are 4.87 ± 0.07 eV and 2.61 ± 0.12 eV, respectively. Using technology computer-aided design simulations, we incorporate our experimental results to estimate the contact resistivity that would be attained at various dielectric layer thicknesses. We find that for achieving the 100 mΩ·cm 2 contact resistivity benchmark, Al 2 O 3 layers should be no thicker than 1.65 nm for a p -type polysilicon-based hole-selective contact, assuming hole tunneling masses taken from the literature. Correspondingly, for HfO 2 and SiO 2 , an upper limit of 1.4 nm is determined as the thickness threshold in order to utilize these ALD-grown layers for contacts in high-performance silicon photovoltaics.
22 December 2022 in IEEE Journal of Photovoltaics
The recombination of photogenerated charge carriers at metal-semiconductor interfaces remains a major source of efficiency loss in photovoltaic cells. Here, we present SiN x and AlO x nanolayers as promising interface dielectrics to enable high efficiency hole selective passivating contacts. It is demonstrated that SiN x deposited via direct plasma enhanced chemical vapour deposition can be grown controllably at thicknesses of 2 nm. The valence band offsets between crystalline silicon and ultrathin AlO x and SiN x nanolayers are measured as 3.5 and 1.4 eV, respectively. This predicts a larger tunnelling current for holes, compared to SiO x used typically. Resistivity measurements show that SiN x and AlO x nanolayers have lower contact resistivities compared to SiO x , with values as low as 100 mΩ·cm 2 . Analysis of the current transport mechanisms confirmed that tunnelling dominates the conduction through SiN x , while a mixture of tunnelling and pinholes are present in the AlO x structure. Lifetime measurements gave initial indications of the passivation quality of the films, with just 10 cycles of AlO x achieving 260 μ s after annealing and 1.9 ms with extrinsic field effect passivation added. Finally, the intrinsic built-in charge in the dielectrics was determined using surface photovoltage measurements and simulations are used to estimate the influence of nanolayer built-in charge in both poly-Si and dopant-free passivating contacts to enable future high efficiency solar cells.