Vadim Skeeba

Dr. Vadim Skeeba

Department of Industrial Machinery Design, Novosibirsk State Technical University, Novosibirsk, Novosibirskaya Oblast’, Russia
orcid

Research Focus & Metrics

Academic Career Length

13Years (2014-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
13 December 2022 in Metals
Verified
Journal Article
Open access
PDF file
VRViktor A. Rezanov
Viktor A. Rezanov
Nikita MartyushevNikita Martyushev
Nikita Martyushev
VKVladislav Kukartsev
Vladislav Kukartsev
Vadim TynchenkoVadim Tynchenko
Vadim Tynchenko
VKViktor A. Kukartsev
Viktor A. Kukartsev
Antonina KarlinaAntonina Karlina
Antonina Karlina
An analysis of the results of rail operation shows that up to a third of all rail breaks in the railway line and up to 12.9% of all withdrawn acute defective rails are associated with welded joints. This is largely explained by the formation of structures with martensite sections in the welded joints of rails and the formation of burns. This work presents the results of studying welded joints, obtained under three welding modes (continuous flash welding, pulsating flash welding and combined flash welding). The conducted studies have shown that the flash welding mode significantly influences both the cooling rate value and the very nature of the thermal cycle of the welded joint as a whole. Changes in the cooling rate under different modes exert a significant influence on the structure and properties of the weld. Resistance welding of rails from the steel grade E76HGF by pulsating flash welding can result in the appearance of needle martensite areas, which is the reason for increased embrittlement of the weld and a decrease in its properties. The conducted field experiments have reliably shown that in the conditions of the combined welding mode it becomes possible to avoid these problems. Moreover, a slight increase in the mechanical properties of the weld in the range of 2–4% has been experimentally recorded, and the destructive load of the welded joint of the rail increases by 2–3% at high values of the bending deflection. In turn, these factors allow a significant reduction in the number of cases of rail welded-joint failures in real conditions of their operation.

21 December 2021 in Applied Sciences
Verified
Journal Article
Open access
PDF file
EEEgor Alekseevich Efremenkov
Egor Alekseevich Efremenkov
Nikita MartyushevNikita Martyushev
Nikita Martyushev
Vadim SkeebaVadim Skeeba
Vadim Skeeba
MGMaria V. Grechneva
Maria V. Grechneva
AOAndrei Olisov
Andrei Olisov
AEAnatoly D. Ens
Anatoly D. Ens
Purpose: In the present work, different combinations of fits and accuracies, in relation to the profiles of mating parts, have been analysed in order to assess the degree of the engagement of transmissions that contain intermediate rolling elements. The aim of this work is to determine which fits have decreased accuracy, but nevertheless provide a minimum manufacturing clearance for the transmission engagement in order to reduce the cost of parts production. Methods and materials: Considering the normal probabilistic distribution law in relation to the obtained dimensions of the manufacturing equipment, a combination of fits were selected using the incomplete interchangeability method, taking into account the peculiarities of the cycloid engagement in transmissions with intermediate rolling elements (IRE). Results: Having studied various combinations of fits of parts that are engaged in transmissions with intermediate rolling elements and a free cage (IREFC), a combination of fits for a “ring, rolling-element cam” were determined, in which a technological clearance of 3 µm is formed in the engagement. At the same time, cycloid disk profiles are manufactured according to the 9th tolerance grade, which reduces the laboriousness and cost of the production. Discussion. When reducing the manufacturing accuracy of cycloid disks, it is possible to obtain both very ample clearances and significant negative allowances. For example, having manufactured a ring with the H9 fit, rolling elements with h6 and a cam with js9, the maximum manufacturing clearance can reach 0.086 mm, while the clearance limits vary from 0.025 mm to 0.061 mm. Additionally, if mating parts are manufactured using a combination of K9-h6-js9 fits, a negative allowance varying from 0.014 mm to 0.026 mm will emerge in the engagement. Both described cases are unacceptable because both ample clearances and large negative allowances will negatively influence the working capacity of the mechanism. However, it is possible to select a combination of fits using the 9th tolerance grade of the basic parts, by which the parts will contact in the range from a small negative allowance of 1 µm to a clearance of 3–4 µm. Furthermore, if this is considered, taking into account the machine settings, it is possible to obtain parts according to the 9th accuracy tolerance grade and, at the same time, provide a clearance in the engagement that is almost equal to zero. Moreover, such a combination of fits is relevant for any transmission with IRE. This is a positive result because it reduces the laboriousness when manufacturing parts and, at the same time, provides high accuracy of the mechanism. Conclusions: It has been established that when lowering the accuracy of manufacturing transmission parts with IRE, both clearances and negative allowances may occur in the engagement, depending on the combination of fits. At the same time, it is possible to select such a combination of fits, by which the parts manufactured according to the 9th tolerance grade, will provide almost zero clearance of the engagement of the transmission. In this way, it is possible to reduce the cost of manufacturing the parts for gears with intermediate rolling elements and, at the same time, maintain a high accuracy of the transmission mechanism.

25 March 2019 in Materials
Verified
Journal Article
Open access
PDF file
AZAnna Zykova
Anna Zykova
Nikita MartyushevNikita Martyushev
Nikita Martyushev
Vadim SkeebaVadim Skeeba
Vadim Skeeba
ZDZadkov Denis
Zadkov Denis
AKAndrey Kuzkin
Andrey Kuzkin
A widespread method exerting the influence on the homogeneous formation of the microstructure and enhancement of strength properties of Al-Si alloys is a modification by super- and nanodispersed particles of different chemical compositions. In spite of the significant advances in the studies of the influence of various modifying compositions on the structure and mechanical properties of casted silumins, the literature contains no data about the influence of nanodispersed W-powder on formation of the structural-phase state and mechanical properties of Al-Si alloys. The paper considers the influence of 0.01–0.5 mass % W nanopowder on the structural-phase state and mechanical properties of an Al-12%Si alloy. It has been established that 0.1 mass % of W is an optimal addition. It results in the uniform distribution of eutectic (α-Al + Si), a 1.5-time decrease in the size of the plates of eutectic Si, a change of the shape of coarse plates (coarse plate-like or acicular) into a fine fibrous one, and an enhancement of the mechanical properties by 16–20%.

1 June 2017 in Key Engineering Materials
Verified
Journal Article
Closed access
PDF file
EZEgor A. Zverev
Egor A. Zverev
Vadim SkeebaVadim Skeeba
Vadim Skeeba
Nikita MartyushevNikita Martyushev
Nikita Martyushev
PSPavel Yu. Skeeba
Pavel Yu. Skeeba
We propose the technique of guaranteed quality wear resistant plasma coatings of high-chromium powder material. The appropriate system of engineering models had to be designed in order to obtain the summarized results, as well as to manage the parameters of quality indicators at all stages of the technological processing procedure. Thus, surface roughness was accepted as a criterion in the model development at the stage of preliminary mechanical processing before spraying coatings. The model of plasma coating process proper takes into account the influence of spraying on the main quality indicators, such as adhesive strength, porosity, and the level of residual stresses. The engineering model of finish abrasive grinding is based on ensuring the desired value of the surface roughness parameter provided the geometric and dimensional accuracy of details was achieved.

27 August 2024 in Applied Sciences
Verified
Journal Article
Open access
PDF file
IAIgbayeva Akzharkyn Akzharkyn
Igbayeva Akzharkyn Akzharkyn
KYKassym Yelemessov
Kassym Yelemessov
Dinara BaskanbayevaDinara Baskanbayeva
Dinara Baskanbayeva
Nikita MartyushevNikita Martyushev
Nikita Martyushev
Vadim SkeebaVadim Skeeba
Vadim Skeeba
TOTatiana Oparina
Tatiana Oparina
To date, composite materials, such as polymer concrete, have found wide application in various industries due to their unique properties combining high strength, resistance to aggressive media and durability. Improving the performance characteristics of polymer concrete is an important task aimed at expanding the areas of its application. One of the promising methods of increasing the strength of this material is the use of various fillers. In this paper, the effect of fillers, based on carbon and basalt fibres, on the mechanical properties of polymer concrete was investigated. The polymer concrete was made of the following components: rubble stone, sand, quartz flour and polyester resin. During the experimental work, the amount of carbon and basalt fibres in the polymer concrete mixture varied from 0 to 6%. Bending and compressive strength tests showed that the addition of carbon and basalt fibres increased these properties. The highest bending and compressive strengths were achieved when carbon fibre contents were up to 1.5%, while basalt fibres provided the highest strengths in the case of around 2%. These results confirmed that carbon fibres had a higher efficiency in strengthening polymer concrete compared to that of basalt fibres. This could be explained by the fact that carbon fibres had a higher tensile strength and modulus of elasticity, which allowed them to better redistribute loads within the composite material. The fibre length for carbon fibre, which gave the maximum increase in properties, was 10–15 mm. For basalt fibre, the maximum bending strength was reached at 20 mm and compressive strength at 10 mm. Increasing the content of carbon fibre above 2% and basalt fibre above 1.5% did not give further increase in mechanical properties. In conclusion, it could be stated that the use of carbon fibres as fillers offered significant advantages in strengthening polymer concrete, opening up opportunities for its use in more demanding conditions and in a wider range of industrial applications.

1 September 2016 in Key Engineering Materials
Verified
Journal Article
Closed access
PDF file
Vadim SkeebaVadim Skeeba
Vadim Skeeba
VIVladimir Ivancivsky
Vladimir Ivancivsky
Nikita MartyushevNikita Martyushev
Nikita Martyushev
DLDmitry V. Lobanov
Dmitry V. Lobanov
NVNikita V. Vakhrushev
Nikita V. Vakhrushev
AZAleksey K. Zhigulev
Aleksey K. Zhigulev
It is impossible to improve the most critical performance properties of machine parts without methods of modifying the surface layer using such concentrated energy as laser, plasma, an electron beam or high-frequency currents. For the rational use of these methods, which are characterized by high heating rates, i.e. about 104 ... 105oC/sec a reliable mechanism for determining the processing modes that ensure the required level of quality characteristics of the hardened surface layer of machine parts, is essential. In this paper, the interrelation between the parameter values of thermal cycles, implemented in the surface layer of steel U8, and the modes of electron beam heating in the atmosphere has been determined.