Cu nanoparticle paste has become one of the alternative materials for conventional high-temperature packaging, but this sintering process is significantly inhibited by copper oxides. In this paper, the activated formic acid atmosphere was used to achieve high-strength Cu–Cu bonding at low temperature. When sintered at a temperature of 275 °C for 30 min with a pressure of 5 MPa, a shear strength of more than 70 MPa was achieved. In contrast to formic acid atmosphere, the hydrogen radicals generated by activated formic acid atmosphere facilitated the rapid evaporation of the solvent during preheating process. Moreover, the hydrogen radicals effectively reduced of the oxides on the surface of the Cu nanoparticle resulting in a higher shear strength. This Cu nanoparticle sintering method has great potential in the field of power device integration in future.
In $_{\text{2}}$ O $_{\text{3}}$ has been recognized as a wide-gap transparent semiconductor oxide with high mobility, in which the oxygen plays an important role in its electronic properties. Here, we investigate the effects of air, O $_{\text{3}}$ and N $_{\text{2}}$ annealing on the electrical characteristics of a-In $_{\text{2}}$ O $_{\text{3}}$ thin film transistors (TFTs) by analyzing the behavior of weakly bonded oxygen (O $_{\text{wb}}$ ), excess oxygen (O $_{\text{ex}}$ ), and oxygen vacancy (V $_{\text{O}}$ ) in the channel layer. X-ray diffraction (XRD) result indicates an amorphous phase of In $_{\text{2}}$ O $_{\text{3}}$ layer after annealing. The oxygen behavior and bonding information before and after annealing of the In $_{\text{2}}$ O $_{\text{3}}$ films are investigated via X-ray photoelectron spectroscopy (XPS) measurements. The a-In $_{\text{2}}$ O $_{\text{3}}$ TFTs with field-effect mobility of 50–60 cm $^{\text{2}}$ /Vs and enhanced reliability are achieved by optimizing channel thickness and annealing conditions in air. The large threshold voltage shifting, reduced mobility, and low ON/OFF ratio of O $_{\text{3}}$ -annealed In $_{\text{2}}$ O $_{\text{3}}$ TFT are attributed to the existence of O $_{\text{ex}}$ . The hump-effect observed in N $_{\text{2}}$ -annealed In $_{\text{2}}$ O $_{\text{3}}$ TFT is attributed to the creation of a parasitic channel with high V $_{\text{O}}$ level above the main channel. The results reveal that O $_{\text{wb}}$ can be removed by thermal treatment, and V $_{\text{O}}$ can be partially filled and stabilized without introducing O $_{\text{ex}}$ by annealing the as-deposited In $_{\text{2}}$ O $_{\text{3}}$ TFTs in air at appropriate condition.
A novel bonding process using Ag agglomerates paste prepared by Ag2O reduction has been proposed, which solved the problem of Cu substrate oxidation in the conventional Ag2O sintering process for Cu–Cu bonding. By applying the Ag agglomerate paste to Ag–Ag bonding, a shear strength of 28.3 MPa at 150 °C was obtained. Further studies showed that the optimum sintering temperature was at 225 °C, and a shear strength of 46.4 MPa was obtained. In addition, a shear strength of 20 MPa was obtained at 225 °C for Cu–Cu bonding. Compared to common Ag pastes, the results in this paper revealed that the sintering behavior of Ag agglomerates was unique, and the sintering mechanisms for Ag–Ag and Cu–Cu bonding were also discussed.
Wafer bonding of a silicon carbide (SiC) diaphragm to a patterned SiC substrate coated with aluminum nitride (AlN) film as an insulating layer is a promising choice to fabricate an all-SiC capacitive pressure sensor. To demonstrate the bonding feasibility, a crystalline AlN film with a root-mean-square (RMS) surface roughness less than ~0.70 nm was deposited on a SiC wafer by a pulsed direct current magnetron sputtering method. Room temperature wafer bonding of SiC-AlN by two surface activated bonding (SAB) methods (standard SAB and modified SAB with Si nano-layer sputtering deposition) was studied. Standard SAB failed in the bonding, while the modified SAB achieved the bonding with a bonding energy of ~1.6 J/m2. Both the microstructure and composition of the interface were investigated to understand the bonding mechanisms. Additionally, the surface analyses were employed to confirm the interface investigation. Clear oxidation of the AlN film was found, which is assumed to be the failure reason of direct bonding by standard SAB.
Oxygen post annealing is a promising method for improving the quality of the SiC metal oxide semiconductor (MOS) interface without the introduction of foreign atoms. In addition, a low oxygen partial pressure annealing atmosphere would prevent the additional oxidation of SiC, inhibiting the generation of new defects. This work focuses on the effect and mechanism of low oxygen partial pressure annealing at different temperatures (900–1250 °C) in the SiO2/SiC stack. N2 was used as a protective gas to achieve the low oxygen partial pressure annealing atmosphere. X-ray photoelectron spectroscopy (XPS) characterization was carried out to confirm that there are no N atoms at or near the interface. Based on the reduction in interface trap density (Dit) and border trap density (Nbt), low oxygen partial pressure annealing is proven to be an effective method in improving the interface quality. Vacuum annealing results and time of flight secondary ion mass spectrometry (ToF-SIMS) results reveal that the oxygen vacancy (V[O]) filling near the interface is the dominant annealing mechanism. The V[O] near the interface is filled more by O2 in the annealing atmosphere with the increase in temperature.