Rechargeable magnesium batteries are promising for future energy storage. However, among other challenges, their practical application is hindered by low coulombic efficiencies of magnesium plating and stripping. Fundamental processes such as the formation, structure, and stability of passivation layers and the influence of different electrolyte components on them are still not fully understood. In this work, we gain unique insights into the initial Mg plating and stripping cycles by comparing magnesium bis(trifluoromethanesulfonyl)imide (Mg(TFSI) 2 )‐ and magnesium tetrakis(hexafluoroisopropyloxy)borate (Mg[B(hfip) 4 ] 2 )‐based electrolytes, each with and without MgCl 2 , on gold electrodes by highly sensitive operando electrochemical quartz crystal microbalance with dissipation monitoring (EQCM−D) applying hydrodynamic spectroscopy. With the stable Mg[B(hfip) 4 ] 2 ‐based electrolytes, highly efficient and interphase‐free cycling is possible and passivation layers are attributed to electrolyte contaminants. These are forming and degrading during the so‐called initial conditioning process. With the more reactive Mg(TFSI) 2 ‐based electrolyte, thick passivation layers with small pores are growing during cycling. We demonstrate that the addition of chloride lowers the amount of passivated Mg deposits in these electrolytes and accelerates the currentless dissolution of the passivation layer. This has a positive effect since we observe the most efficient cycling and uniform deposition when no interphase is present on the electrode.
7 December 2022 in Angewandte Chemie International Edition
For sustainable energy storage, all‐organic batteries based on redox‐active polymers promise to become an alternative to lithium ion batteries. Yet, polymers contribute to the goal of an all‐organic cell as electrodes or as solid electrolytes. Here, we replace the electrolyte with a deep eutectic solvent (DES) composed of sodium bis(trifluoromethanesulfonyl)imide (NaTFSI) and N‐methylacetamide (NMA), while using poly(2,2,6,6‐tetramethylpiperidin‐1‐yl‐oxyl methacrylate) (PTMA) as cathode. The successful combination of a DES with a polymer electrode is reported here for the first time. The electrochemical stability of PTMA electrodes in the DES at the eutectic molar ratio of 1 : 6 is comparable to conventional battery electrolytes. More viscous electrolytes with higher salt concentration can hinder cycling at high rates. Lower salt concentration leads to decreasing capacities and faster decomposition. The eutectic mixture of 1 : 6 is best suited uniting high stability and moderate viscosity.
Sustainable battery concepts are of great importance for the energy storage demands of the future. Organic batteries based on redox‐active polymers are one class of promising storage systems to meet these demands, in particular when combined with environmentally friendly and safe electrolytes. Deep Eutectic Solvents (DESs) represent a class of electrolytes that can be produced from sustainable sources and exhibit in most cases no or only a small environmental impact. Because of their non‐flammability, DESs are safe, while providing an electrochemical stability window almost comparable to established battery electrolytes and much broader than typical aqueous electrolytes. Here, we report the first all‐organic battery cell based on a DES electrolyte, which in this case is composed of sodium bis(trifluoromethanesulfonyl)imide (NaTFSI) and N‐methylacetamide (NMA) alongside the electrode active materials poly(2,2,6,6‐tetramethylpiperidin‐1‐yl‐oxyl methacrylate) (PTMA) and crosslinked poly(vinylbenzylviologen) (X‐PVBV2+). The resulting cell shows two voltage plateaus at 1.07 V and 1.58 V and achieves Coulombic efficiencies of 98 %. Surprisingly, the X‐PVBV/X‐PVBV+ redox couple turned out to be much more stable in NaTFSI : NMA 1 : 6 than the X‐PVBV+/X‐PVBV2+ couple, leading to asymmetric capacity fading during cycling tests.
23 August 2021 in Angewandte Chemie International Edition
While numerous reference electrodes suitable for aqueous electrolytes exist, there is no well‐defined standard for non‐aqueous electrolytes. Furthermore, reference electrodes are often large and do not meet the size requirements for small cells. In this work, we present a simple method for fabricating stable 3D‐printed micro‐reference electrodes. The prints are made from polyvinylidene fluoride, which is chemically inert in strong acids, bases, and commonly used non‐aqueous solvents. We chose six different reference systems based on Ag, Cu, Zn, and Na, including three aqueous and three non‐aqueous systems to demonstrate the versatility of the approach. Subsequently, we conducted cyclic voltammetry experiments and measured the potential difference between the aqueous homemade reference electrodes and a commercial Ag/AgCl‐electrode. For the non‐aqueous reference electrodes, we chose the ferrocene redox couple as an internal standard. From these measurements, we deduced that this new class of micro‐reference electrodes is leak‐tight and shows a stable electrode potential.
Rechargeable magnesium batteries could provide future energy storage systems with high energy density. One remaining challenge is the development of electrolytes compatible with the negative Mg electrode, enabling uniform plating and stripping with high Coulombic efficiencies. Often improvements are hindered by a lack of fundamental understanding of processes occurring during cycling, as well as the existence and structure of a formed interphase layer at the electrode/electrolyte interface. Here, a magnesium model electrolyte based on magnesium bis(trifluoromethanesulfonyl)imide (Mg(TFSI)2) and MgCl2 with a borohydride as additive, dissolved in dimethoxyethane (DME), was used to investigate the initial galvanostatic plating and stripping cycles operando using electrochemical quartz crystal microbalance with dissipation monitoring (EQCM‐D). We show that side reactions lead to the formation of an interphase of irreversibly deposited Mg during the initial cycles. EQCM‐D based hydrodynamic spectroscopy reveals the growth of a porous layer during Mg stripping. After the first cycles, the interphase layer is in a dynamic equilibrium between the formation of the layer and its dissolution, resulting in a stable thickness upon further cycling. This study provides operando information of the interphase formation, its changes during cycling and the dynamic behavior, helping to rationally develop future electrolytes and electrode/electrolyte interfaces and interphases.
Copper electrodeposition on Au(111) from deep eutectic solvents (DESs) type III was investigated employing cyclic voltammetry as well as chronoamperometry. It was further examined on Au(poly) using the electrochemical quartz crystal microbalance (EQCM). The employed DESs are mixtures of choline chloride (ChCl) or choline nitrate (ChNO3) with ethylene glycol (EG) as hydrogen bond donor (HBD), each in a molar ratio of 1 : 2. CuCl, CuCl2, or Cu(NO3)2 ⋅ 3H2O were added as copper sources. Underpotential deposition (UPD) of Cu precedes bulk deposition in chloride as well as nitrate electrolytes. Cu deposition from Cu+ in chloride media is observed as a one‐electron reaction, whereas deposition from Cu2+ occurs in two steps since Cu+ is strongly stabilized by chloride. Cu+ is less stabilized by nitrate and the beginning of bulk deposition in the nitrate‐containing DES with Cu2+ is shifted by several hundred mV to more positive potentials compared to the chloride DES. A diffusion‐controlled, three‐dimensional nucleation and growth mechanism is found by chronoamperometric measurements and analysis based on the model of Scharifker and Mostany.