The presented work deals with the investigation of mechanical tribological properties on Inconel 625 superalloy, which is welded on a 16Mo3 steel pipe. The wall thickness of the basic steel pipe was 7 mm, while the average thickness of the welded layer was 3.5 mm. The coating was made by the cold metal transfer (CMT) method. A supercritical bending of 180° was performed on the material welded in this way while cold. The mechanical properties evaluated were hardness, wear resistance, coefficient of friction (COF) and change in surface roughness for both materials. The UMT Tribolab laboratory equipment was used to measure COF and wear resistance by the Ball-on-flat method, which used a G40 steel pressure ball. The entire process took place at an elevated temperature of 500 °C. The measured results show that the materials after bending are reinforced by plastic deformation, which leads to an increase in hardness and also resistance to wear. Superalloy Inconel 625 shows approximately seven times higher rate of wear compared to steel 16Mo3 due to the creation of local oxidation areas that support the formation of abrasive wear and do not create a solid lubricant, as in the case of steel 16Mo3. Strain hardening leads to a reduction of possible wear on Inconel 625 superalloy as well as on 16Mo3 steel. In the case of the friction process, the places of supercritical bending of the structure showed the greatest resistance to wear compared to the non-deformed structure.
This article presents a comparative study of WC and CrC coatings deposited by the plasma-enhanced chemical vapor method using the hexacarbonyls of W and Cr as precursors. The measured thicknesses of the WC and CrC coatings are equal to ca. 1.5 µm. The WC coating consists of microcolumns with a conical end, with gaps between the microcolumns up to approximately 100 nm, and their structure is formed by nanoparticles in the shape of globules with a diameter of up to 10 nm. In the case of the CrC coating, a cauliflower structure with gaps ranging from 20 to 100 nm was achieved. The diameter of cauliflower grains is from 50 nm to 300 nm. The C content in the WC and CrC coating is 66.5 at.% and 75.5 at.%. The W content is 1.4 at.% and the Cr content in the CrC coating is 1.2 at.%. The hardness and Young’s modulus of the WC coating are equal to 9.2 ± 1.2 GPa 440.2 ± 14.2 GPa, respectively. The coefficients of friction and wear volume of the WC coating are equal to 0.7 and −1.6 × 106/+3.3 × 106 µm3, respectively. The hardness and Young’s modulus of the CrC coating are 7.5 ± 1.2 GPa and 280 ± 18.5 GPa, respectively. The coefficients of friction and wear volume of the CrC coating are 0.72 and −18.84 × 106/+0.35 × 106 µm3, respectively.
This study examines the impact of varying pulse conditions on the properties of titanium diboride (TiB2) coatings deposited by high-power impulse magnetron sputtering (HiPIMS). The coatings were prepared on steel substrates using an industrial-scale system. During the experiments, the HiPIMS frequency and pulse width were systematically varied to examine their influence on the coating’s microstructural, mechanical, and tribological properties. The obtained results show a correlation between process parameters and coating performance. A maximum hardness of 39.7 GPa and a coefficient of friction (CoF) as low as 0.68 were achieved. The best combination of mechanical properties was observed for coatings prepared in a frequency range of 600–1000 Hz and with a pulse width of 50 µs. Notably, the optimal tribological properties and surface roughness were obtained at 800 Hz and a 50 µs pulse width. This work demonstrates that fine-tuning HiPIMS pulse conditions is crucial for achieving high-quality TiB2 coatings with enhanced functional performance.
The temperature dependence of tensile characteristics and fracture toughness of the standardly heat-treated low-alloyed steel OCHN3MFA along with three additionally heat-treated grades was experimentally studied. In the temperature range of ⟨−196; 22⟩ °C, all the additional heat treatments transferred the standard steel from a high- to ultra-high strength levels even with improved tensile ductility characteristics. This could be explained by a reduction of the inclusion content, refinement of the martensitic blocks, ductile retained austenite content, and homogenization of the shape ratio of martensitic laths as revealed by metallographic, X-ray, and EBSD techniques. On the other hand, the values of the fracture toughness of all grades were found to be comparable in the whole temperature range as the cause of a high stress triaxiality in the pre-cracked Charpy V-notch samples. The values of the fracture toughness of the standard steel grade could be predicted well using the fracture model proposed by Pokluda et al. based on the tensile characteristics. Such a prediction failed in the case of additionally heat-treated grades due to the different temperature dependence of the fracture mechanisms occurring in the tensile and fracture-toughness tests. While the tensile samples fractured in a ductile-dimple mode at all temperatures, the fracture-toughness specimens exhibited a transition from the ductile to quasi-brittle fracture mode with decreasing temperature. This transition could be interpreted in terms of a transfer from the model proposed by Rice and Johnson to the model of Tvergaard and Hutchinson.
The diffusion aluminide coatings are used for high-temperature applications. Structural materials of particular components degrade during service due to fatigue, creep, oxidation, corrosion and erosion. The requirements of higher efficiency of modern industrial applications increase the development of new structural materials, technologies and protective coatings. Properties of many structural materials such ultimate tensile strength, creep strength and fatigue are generally optimized for maximum high-carrying loading with less emphasis on environmental resistance. For these applications, the performance characteristics are limited by the operating conditions, which can be tolerated by the used materials. The main structural materials for high mechanical and thermal loading are superalloys protected against aggressive environment by coatings. Cyclic oxidation is the superposition of thermal cycles in an oxidation environment. The main goal of the experimental work was to compare the cyclic oxidation of protective Al and AlSi coatings deposited on both Inconel 713 LC and MAR-M247 superalloys. The resulting graph revealed that samples from IN 713 LC without coating show good resistance and their mass change is maintained above zero limit. Samples from MAR 247 LC with both Al and AlSi coatings appear to be the most acceptable selection of combination relating to superalloys/coating.