The V-defect is a naturally occurring inverted hexagonal pyramid structure that has been studied in GaN and InGaN growth since the 1990s. Strategic use of V-defects in pre-quantum well superlattices or equivalent preparation layers has enabled record breaking efficiencies for green, yellow, and red InGaN light emitting diodes (LEDs) utilizing lateral injection of holes through the semi-polar sidewalls of the V-defects. In this article, we use advanced characterization techniques such as scattering contrast transmission electron microscopy, high angle annular dark field scanning transmission electron microscopy, x-ray fluorescence maps, and atom probe tomography to study the active region compositions, V-defect formation, and V-defect structure in green and red LEDs grown on (0001) patterned sapphire and (111) Si substrates. We identify two distinct types of V-defects. The “large” V-defects are those that form in the pre-well superlattice and promote hole injection, usually nucleating on mixed (Burgers vector b=±a±c) character threading dislocations. In addition, “small” V-defects often form in the multi-quantum well region and are believed to be deleterious to high-efficiency LEDs by providing non-radiative pathways. The small V-defects are often associated with basal plane stacking faults or stacking fault boxes. Furthermore, we show through scattering contrast transmission electron microscopy that during V-defect filling, the threading dislocation, which runs up the center of the V-defect, will “bend” onto one of the six {101¯1} semi-polar planes. This result is essential to understanding non-radiative recombination in V-defect engineered LEDs.
Micro-light-emitting diodes (µLEDs) are gathering significant interest as a technology for emerging micro-displays. However, µLEDs encounter numerous obstacles, including size-dependent efficiency loss, poor efficiency of red µLEDs, and challenges associated with the mass transfer and integration of full-color µLEDs. These issues become more acute in ultra-small µLEDs (<5 µm), which were required by the augmented reality (AR) displays. Here, we discuss the principal challenges faced by µLEDs and explore the possible solutions. We highlight recent advances in InGaN-based RGB µLEDs tailored for AR displays. In particular, we discuss the advancements in ultra-small InGaN µLEDs scaled down to 1 µm, the developments in InGaN red µLEDs, and the implementation of tunnel junction-based cascaded InGaN µLEDs for monolithic integration.
We report on the material challenges of the growth of highly conductive n-AlGaN in germicidal ultraviolet light emitting diodes (GUV LEDs), with the degradation of the surface morphology of thick highly doped n-AlGaN due to the Si anti-surfactant effect. Threading dislocation inclination, increasing relaxation, and eventual cracking were observed with epitaxial n-AlGaN films thicker than 400 nm, along with an increasing Ga composition with the same metalorganic flows. With the optimization of the n-AlGaN conductivity in previous works, thin n-AlGaN films with high conductivity along with a smoothing superlattice were incorporated in GUV LED devices, resulting in LEDs with 285 nm electroluminescence, a low forward voltage of 4.2 V with a peak external quantum efficiency (EQE) of 10.6% and a peak wall-plug efficiency of 8.6% below 1 A/cm2, and an EQE of 5.5% at 20 A/cm2.
We report a selective electrochemical etching-based liftoff technique for III-nitride thin films using a heavily Si-doped sacrificial layer. This method enables the detachment of the millimeter-sized III-nitride thin films with tunable thickness from arbitrary substrates, achieving minimal damage and sub-nanometer liftoff surface roughness, offering more flexibility than traditional liftoff methods such as laser liftoff. Structure and optical characterization confirm the preservation of the crystal quality throughout the process. Notably, InGaN-based blue μLEDs were lifted off and transferred onto Si substrates, maintaining excellent optoelectronic properties, showing great potential in mass transfer of nitride-based μLEDs for micro-display. This proof-of-concept demonstration highlights a scalable, low-damage pathway for heterogeneous integration of III-nitride materials onto diverse platforms for advanced optoelectronic applications.
Efficiencies exceeding 40% have already been achieved with GaAs-based multijunction (MJ) solar cells. In this talk, we will discuss the unique advantages and challenges of fabricating hybrid InGaN-GaAs MJ cells for ultrahigh efficiency device designs.
Investigation of the growth and properties of binary ScN can aid in the understanding of its ferroelectric ternary alloys with GaN and AlN, but there are no existing data for ScN grown by metalorganic chemical vapor deposition (MOCVD). In this work, ScN growth by MOCVD was demonstrated using the Sc precursor (EtCp)2Sc(dbt). A broad range of growth temperatures, pressures, and V/III ratios were tested to investigate the impact of growth parameters on the properties of MOCVD-grown ScN. Approximately 100 nm-thick ScN films with growth rates from 0.06 to 0.20 Å/s were deposited on c-sapphire, (0001) GaN, Si-face 4H-SiC, and (001) Si. X-ray diffraction measurements showed that ScN films were solely (111)-oriented on both sapphire and GaN. Hall effect measurements revealed very high n-type electrical charge in the samples. The carrier concentrations of ScN on sapphire ranged from 2.1 × 1020 to 7.2 × 1020 cm−3, with electron mobilities in the range of 20–7 cm2 V−1 s−1. ScN films on GaN exhibited carrier concentrations from 9.6 × 1019 to 2.5 × 1020 cm−3 and electron mobilities from 42 to 8.5 cm2 V−1 s−1. The lowest sheet resistance of 45 Ω/□ (resistivity of 5.2 × 10−4 Ω-cm) was achieved for an ScN on sapphire film. These results indicate the potential for integrating ScN into the next generation of nitride electronics through MOCVD growth.