An absorber with a high absorbing efficiency is crucial for X-ray transition edge sensors (TESs) to realize high quantum efficiency and the best energy resolution. Semimetal Bismuth (Bi) has shown greater superiority than gold (Au) as the absorber due to the low specific heat capacity, which is two orders of magnitude smaller. The electroplating process of Bi films is investigated. The Bi grains show a polycrystalline rhombohedral structure, and the X-ray diffraction (XRD) patterns show a typical crystal orientation of (012). The average grain size becomes larger as the electroplating current density and the thickness increase, and the orientation of Bi grains changes as the temperature increases. The residual resistance ratio (RRR) (R300 K/R4.2 K) is 1.37 for the Bi film (862 nm) deposited with 9 mA/cm2 at 40 °C for 2 min. The absorptivity of the 5 μm thick Bi films is 40.3% and 30.7% for 10 keV and 15.6 keV X-ray radiation respectively, which shows that Bi films are a good candidate as the absorber of X-ray TESs.
In this work, the interface composition of the superconducting Ti/PdAu bilayer is tuned by an annealing process in N2 from 100 to 500 °C to control the superconducting transition temperature (Tc). This Ti-PdAu composition layer is characterized with a high-resolution transmission electron microscopy (HRTEM) and energy-dispersive spectrometer (EDS) to show the infiltration process. The surface topography, electrical, and cryogenic properties are also shown. The inter-infiltration of Ti and PdAu induced by the thermal treatments generates an intermixed layer at the interface of the bilayer film. Due to the enforced proximity effect by the annealing process, the Tc of Ti (55 nm)/PdAu (60 nm) bilayer thin films is tuned from an initial value of 243 to 111 mK which is a temperature that is suitable for the application as the function unit of a superconducting transition edge sensor.
30 March 2023 in IEEE Transactions on Applied Superconductivity
The critical temperature ( T c) of superconducting Ti/Au bilayer films is crucial for the performance of transition-edge sensors. We use a co-sputtering technique to insert a Ti-Au mixture layer as an artificial diffusion layer between a supercon-ducting Ti film and a normal Au bilayer. The Ti-Au mixture layers have different thicknesses and component ratios. The cross-section and element information of thin films was characterized by a high-resolution transmission electron microscopy (HRTEM) and energy dispersive X-ray spectroscopy (EDS). The variation of T c is meas-ured for a series of Ti/Ti-Au/Au films. T c is related to both the thickness and Ti-Au ratio in the mixture layer. We attempt to model the T c variation based on the Usadel theory with an equiva-lent thickness ratio.
Due to its highly unreactive nature and advanced biocompatibility, niobium (Nb) coating films are increasingly being used to improve the corrosion resistance and biocompatibility of base implant materials. However, Nb films have relatively low yield strengths and surface hardness; therefore, it is necessary to explore a simple and low-cost method to improve their mechanical properties. Magnetron sputtering is a commonly used tool for Nb film deposition. Applying substrate bias can introduce Ar+ bombard to the film surface, which is effective to improve the film’s mechanical properties. As the direct current (DC) bias-sputtering tool requires an extra DC power supply, applying the negative bias by a radio frequency (RF) power source (usually installed in the sputtering system to conduct substrate pre-cleaning) will be more economical and convenient. Moreover, the RF bias was accompanied with higher ion density and energy compared to the DC bias. In this study, Nb films were deposited on silicon wafers by magnetron sputtering under different RF bias powers. The effects of the RF bias on the structural parameters and mechanical properties of the films were studied via stress measurements, X-ray diffraction, and indentation tests. The results show that the RF bias can change the crystal distribution, grain size, and lattice parameter of the film, as well as the mechanical properties. The stress of the Nb film was compressive; it increased markedly when an RF power was applied and saturated when the RF power was over 40 W. The hardness of the film increased from 4.17 GPa to 5.34 GPa with an elevating RF power from 0 W to 60 W. This study aimed to enhance the mechanical properties of the Nb films deposited by RF-biased sputtering, which provides wider potentials for Nb film as protective coatings for medical–biological implant bodies. Although the research was carried out on Si substrates to facilitate the study of film stress, we believe that the evolution trends of our results will also apply to other metal substrates, because the measured film mechanical properties are intrinsic.
Superconducting transition-edge sensors (TESs) exhibit excellent single-photon detection performance. The quantum efficiency (QE), which quantifies the probability that an incident photon is absorbed and converted into a measurable signal, is strongly governed by the optical properties of the constituent thin films. Specifically, for typical TES device architectures where optical transmission is negligible, maximizing the QE requires the minimization of surface reflectance to ensure high photon absorptance. In this work, we systematically study how anodic oxidation modifies the optical response of superconducting titanium (Ti) thin films that are relevant for TES devices. Anodization is carried out under well-controlled constant-current conditions in an aqueous electrolyte containing ammonium pentaborate and ethylene glycol. Experimentally, we show that anodic oxidation substantially reduces the ultraviolet (UV) reflectance and induces a monotonic redshift of the reflectance minimum as the anodic oxidation cutoff voltage (Vocv) increases. Finite-difference time-domain (FDTD) simulations based on spectroscopic ellipsometry data reproduce the measured spectra with good fidelity for most samples, validating the extracted optical constants. By comparing samples prepared at different current densities and oxidation times, we identified Vocv as the primary parameter controlling the reflectance response, because it determines the thickness and effective optical properties of the anodic TiOx layer. Under optimized conditions, reflectance values below 1% in the 320.9–340.2 nm wavelength range and below 2% in the 316.3–346.3 nm range are achieved, indicating a significant enhancement in potential absorptance. These results demonstrate that anodic oxidation provides a simple, post-fabrication, and voltage-tunable route for engineering the UV optical response of Ti-based TES structures and for enhancing their potential QE by suppressing reflection losses.
24 February 2022 in IEEE Transactions on Applied Superconductivity
High quality superconducting films are crucial for the develop-ment of transition edge sensors (TESs) with high energy resolu-tion ability. Controlling the superconducting transition tempera-ture (Tc) and the transition width (Tc) of the films from the su-perconducting to normal metal state is important for the per-formance of TESs. We present a new kind of superconducting Ti/PdAu bilayer film. The influence of Ti/PdAu thickness ratio on Tc through the proximity effect is investigated. The Tc can be tuned from 175 mK to 336 mK by setting the PdAu thickness to 60 nm and varying the thickness of Ti from 50 nm to 70 nm. The minimum Tc is ~ 1 mK. The element distribution at the inter-face between the Ti and PdAu layers has been analyzed by a high-resolution transmission electron microscopy (HRTEM), energy-dispersive spectrometer (EDS) and X-ray diffraction (XRD). Roughness, electrical resistivity, and cryogenic proper-ties are also shown. The superconducting Ti/PdAu bilayer film shows a great promise as a new material for TESs.