This article reports on two generations of GaN-on-sapphire super-heterojunction (SHJ) transistors, aiming at the realization of 10-kV class power transistors with low static and dynamic ON-resistance. First generation (Gen. 1) GaN SHJ-FETs used a single 2-D electron gas (2DEG) channel design with Schottky gate. Experimental results indicated the feasibility of achieving 10-kV blocking, however, room for improvement to reduce static source-to-drain ON-resistance ${R}_{\text {DS},\text {ON}}$ and dynamic ${R}_{\text {DS},\text {ON}}$ degradation. A second generation (Gen. 2) SHJ-MOSFET was designed using an epitaxy with two 2DEG channels for larger ON-state drain current and smaller ${R}_{\text {DS},\text {ON}}$ . The high-voltage capability and dynamic ${R}_{\text {DS},\text {ON}}$ degradation mitigation were reached by implementing the GaN SHJ design, while simultaneously avoiding surface trapping between the gate and the SHJ structure. Gen. 2 experimentally showed scaling of blocking voltage with SHJ length up to 10 kV, reduced static ${R}_{\text {DS},\text {ON}}$ of $71.4~\Omega \cdot $ mm (73.5 $\text{m}\Omega \cdot $ cm $^{{2}}{)}$ , low ${R}_{\text {DS,ON}}{C}_{\mathrm {O(}\mathrm {tr})}$ of ~4.9 ps, and controlled current collapse of 123% when switched from an OFF-state bias of 3 kV.
This letter reports an experimental demonstration of charge-balanced GaN super-heterojunction Schottky barrier diodes (SHJ-SBDs). Charge balance between the n-type delta-doping and the p-type doping was achieved by adjusting the thickness of the pGaN. This device structure enabled scaling of breakdown voltage to over 3 kV, and dynamic switching up to 2.8 kV without using any field-plate.
24 September 2021 in IEEE Transactions on Electron Devices
This article reports GaN super-heterojunction Schottky barrier diodes (SHJ-SBDs) with substantially improved performance. Metal-2DEG sidewall n-ohmic contacts were deployed to achieve low contact resistance of $0.75~\Omega ~ \cdot ~mm$ , avoiding the risk of abnormally high contact resistance caused by inaccurate etch depth control. A pGaN notch formed near the cathode successfully eliminated excessive hole conduction caused by the sidewall n-ohmic contact. Isolation was improved by a high-energy Al implantation step. The resulting SHJ-SBD exhibited a breakdown voltage (BV) of ~12.5 kV and a specific resistance of 100.8 $\text{m}\Omega ~ \cdot ~cm^{2}$ .
15 March 2022 in IEEE Transactions on Electron Devices
This article presents the static and dynamic characterization of 4.2-kV super-junction p-n diodes at high temperatures. Reduction of the forward current with increasing temperature is consistent with 2DEG mobility degradation caused by polar optical phonon scattering. Reverse leakage current was dominated by isolation leakage, with an activation energy of ~0.26 eV, close to the reported activation energy of surface leakage. Dynamic switching characterization in the temperature range from room temperature (RT) to 300 °C showed a nonmonotonic dependence of dynamic ON-resistance on temperature. At room temperature and 50 °C, devices showed zero current collapse (CC) up to OFF-state stress bias of 3 kV at 100 $\mu \text{s}$ timescale. Between 100 °C and 200 °C, significant CC was observed. From 250 °C to 300 °C, devices showed recovery from the severe CC. The degradation and recovery of dynamic ON-resistance can be explained by emission and recapture of holes during the OFF- and ON-states, respectively.
Physics-based 3D simulations were conducted on a GaN high-electron-mobility transistor (HEMT) and a super-heterojunction field-effect transistor (SHJFET) to investigate the single event effect mechanism under heavy ion irradiation. Most of the single event transient current in HEMT was attributed to the punch-through effect in the bulk caused by the local increase in electrostatic potential. With improved E-field management and a more favorable potential profile to suppress source electron injection, the SHJFET had a 70% lower transient current peak value compared to the HEMT.
The reliability of GaN-based devices operating under high temperatures is crucial for their application in extreme environments. To identify the fundamental mechanisms behind high-temperature degradation, we investigated GaN-on-sapphire Schottky barrier diodes (SBDs) under simultaneous heating and electrical biasing. We observed the degradation mechanisms in situ inside a transmission electron microscope (TEM) using a custom-fabricated chip for simultaneous thermal and electrical control. The pristine device exhibited a high density of extended defects, primarily due to lattice mismatch and thermal expansion differences between the GaN and sapphire. TEM and STEM imaging, coupled with energy-dispersive X-ray spectroscopy (EDS), revealed the progressive degradation of the diode with increasing bias and temperature. At higher bias levels (4–5 V) and elevated temperatures (300–455 °C), the interdiffusion and alloying of the Au/Pd Schottky metal stack with GaN, along with defect generation near the interface, resulted in Schottky contact failure and catastrophic device degradation. A geometric phase analysis further identified strain localization and lattice distortions induced by thermal and electrical stresses, which facilitated diffusion pathways for rapid metal atom migration. These findings highlight that defect-mediated electrothermal degradation and interfacial chemical reactions are critical elements in the high-temperature failure physics of GaN Schottky diodes.